Stress corrosion cracking (SCC) in EUROFER RAFM steel subjected to Li-ceramics at 550 °C

Publication date: December 2025

Source: Nuclear Materials and Energy, Volume 45

Author(s): M. Roldán, T. Hernández, F.J. Sánchez

​Publication date: December 2025Source: Nuclear Materials and Energy, Volume 45Author(s): M. Roldán, T. Hernández, F.J. Sánchez  